Cobalt

Property:

Cobalt metal is silver-white metal. Its melting point is 1495 ℃ and boiling point is 
2870 ℃. Hard, with scalability, and its hardness and ductility is stronger than iron. 
Cobalt alloy can maintain their original strength and other valuable properties at high temperatures .

Use:

Used in the manufacturing of cathode x rays tubes and some special products. 
Great mass of cobalt was used in the manufacturing of alloy, such as refractory 
alloy, cemented carbide, welding alloy, as well as a variety of cobaltic alloy steel.

Grade Co9995
Co(%min) 99.95
Impurities
(%max)
C 0.005
S 0.001
Mn 0.005
Fe 0.004
NI 0.02
Cu 0.003
As 0.0005
Pb 0.0004
Zn 0.002
Si 0.003
Cd 0.0003
Mg 0.002
P 0.001
Al 0.002
Sn 0.0003
Sb 0.0003
Bi 0.0003
总  量 0.05
TOTAL

Previous:No Information

Next:No Information

Back

About Us
About Us
Corporate Culture
Qualification Honor
Company Product
Hydrogen Storage Alloys Used for NI-MH battery
Hydrogen Storage Alloys Used for Hydrogen Storage Device
Metal Hydride Hydrogen Storage Device
Accessories
Metal Hydride Hydrogen Storage and Purification Devices
Metal Hydride Hydrogen Compressor
Hydrogen Generator
Ultra-High Purity Hydrogen Generator
News
Contact Us
Contact Us
Feedback
Map

COPYRIGHT © 2016   Whole Win (Beijing) Materials Sci. & Tech. Co., Ltd.   All Right Reserved.    Support:WebQd